Physical salt attack on concrete: mechanisms, influential factors and mitigation

dc.contributor.authorSakr, Mohamed Ramadan Yousef
dc.contributor.examiningcommitteeEl-Salakawy, Ehab (Civil Engineering) Ojo, Olanrewaju (Mechanical Engineering) Shehata, Medhat (Civil Engineering, Ryerson University)en_US
dc.contributor.supervisorBassuoni, Mohamed (Civil Engineering)en_US
dc.date.accessioned2020-09-14T18:39:22Z
dc.date.available2020-09-14T18:39:22Z
dc.date.copyright2020-09-08
dc.date.issued2020-07en_US
dc.date.submitted2020-09-08T15:36:51Zen_US
dc.degree.disciplineCivil Engineeringen_US
dc.degree.levelDoctor of Philosophy (Ph.D.)en_US
dc.description.abstractPhysical salt attack (PSA) is a key damage mechanism of concrete serving in salt-rich media under certain environments; yet, there is still lack of essential knowledge in the technical literature regarding different aspects of PSA. This thesis applied the response surface method to assess the influence of perspective- and performance-based parameters on PSA of 52 concrete mixtures. Also, the research program considered additional parameters that may alter the kinetics of PSA in service by adopting a holistic testing approach of concurrently exposing concrete to PSA and carbonation, simulating elements serving in heavy traffic and industrial zones. In addition, several surface treatments of concrete were tested/developed (nanocomposites) for mitigating PSA and also tested under salt-frost scaling to generalize their applicability. The results suggested limiting the water-to-binder ratio and binder content to a maximum and minimum of 0.40 and 400 kg/m3, respectively, regardless of the binder type. With extended curing, the use of fly ash or slag was beneficial at dosages below 25 and 30%, respectively, for binary binders and 35% for ternary blends combining both. Blended binders (28 to 35% replacement) comprising silica fume (≥ 8%) were capable of resisting severe PSA conditions. Mutual PSA and carbonation escalated the rate of surface scaling compared to single PSA. The wicking factor of concrete informatively captured the trends of damage for single and combined modes. Thermal, mineralogical, and microscopy analyses elucidated the coexistence of complex degradation processes in concrete subjected to combined PSA and carbonation, which was fundamentally different from salt crystallization in case of single PSA. Epoxy, ethyl silicate, and acrylic emulsion coatings protected concrete from PSA. Colloidal nano-silica (50% concentration) minimized PSA and salt-frost scaling. Silane mixed with 5% nano-clay or nano-silica mitigated PSA and salt-frost scaling damage of sound and pre-cracked concrete, with relatively better performance for nano-clay. Methyl-methacrylate/nanocomposites, at 5% dosage, were efficient at resisting PSA, but failed against salt-frost scaling. The synoptic outcomes from this thesis can be used as a basis for updating stipulations on PSA in the current ACI 201.2R document with limits on mixture design variables and suitable surface treatments for concrete protection against PSA.en_US
dc.description.noteFebruary 2021en_US
dc.identifier.citationSakr, M. R., Bassuoni, M. T., & Taha, M. R. (2019). Effect of Coatings on Concrete Resistance to Physical Salt Attack. ACI Materials Journal, 116(6).en_US
dc.identifier.citationSakr, M. R., & Bassuoni, M. T. (2020). Effect of Nano-Based Coatings on Concrete under Aggravated Exposures. Journal of Materials in Civil Engineering, 32(10), 04020284.en_US
dc.identifier.citationSakr, M.R., Bassuoni, M.T., Hooton, D., Drimalas, T., Haynes, H., & Folliard, K.J. Physical Salt Attack on Concrete: Mechanisms, Influential Factors, and Protection. ACI Materials Journal. (Accepted in Jun. 2020, In-press)en_US
dc.identifier.citationSakr, M.R., Bassuoni, M.T., & Ghazy, A. Durability of Concrete Superficially Treated with Nano-silica and Silane/Nano-clay Coatings. Transportation Research Record. (Accepted in June. 2020, In-press)en_US
dc.identifier.citationSakr, M.R., & Bassuoni, M.T. Silane and Methyl-methacrylate based Nanocomposites as Coatings for Concrete Exposed to Salt Solutions and Cyclic Environments. Cement and Concrete Composites. (Submitted in Mar. 2020, Under Review)en_US
dc.identifier.citationSakr, M.R., & Bassuoni, M.T. Modeling of Parameters Affecting Physical Salt Attack of Concrete. ACI Materials Journal. (Submitted in May 2020, Under Review)en_US
dc.identifier.citationSakr, M.R., & Bassuoni, M.T. Performance of Concrete under Physical Salt Attack Combined with Carbonation. Cement and Concrete Research. (Submitted in July 2020, Under Review)en_US
dc.identifier.citationSakr, M.R., & Bassuoni, M.T. (2018) Surface Treatments for Concrete Under Physical Salt Attack. 6th International Conference on Durability of Concrete Structures (ICDCS), Leeds, UK, July 2018en_US
dc.identifier.urihttp://hdl.handle.net/1993/35065
dc.language.isoengen_US
dc.rightsopen accessen_US
dc.subjectPhysical salt attacken_US
dc.subjectConcrete durabilityen_US
dc.subjectSurface treatmentsen_US
dc.subjectPolymeric nanocompositesen_US
dc.subjectSalt-frost scalingen_US
dc.subjectResponse surface methoden_US
dc.titlePhysical salt attack on concrete: mechanisms, influential factors and mitigationen_US
dc.typedoctoral thesisen_US
Files
Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
PhD_Thesis_Mohamed_Sakr_2020.pdf
Size:
11.47 MB
Format:
Adobe Portable Document Format
Description:
PhD Thesis File
License bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
2.2 KB
Format:
Item-specific license agreed to upon submission
Description: