dc.description.abstractPurpose: To evaluate the in vitro shear bond strength (SBS) of orthodontic attachments using 2 self-etching primers (SEP): iBOND and G-Bond. Methods: 180 molars were randomly divided into 12 groups. Teeth were bonded with a stainless steel button using Transbond XT composite. The bonding agents were iBOND, G-Bond, Transbond Plus SEP and Transbond XT primer (control). SBS’s immediately, 24hours and 3months were measured with their Adhesive Remnant Index (ARI). Results: Transbond XT primer (11.22MPa) had a significantly higher immediate SBS than Transbond Plus SEP (5.32MPa), iBOND (6.69MPa) and G-Bond (8.30MPa). 24 hours, Transbond XT primer (16.65MPa) and Transbond Plus SEP (13.20MPa) had a significant increase in their SBS. No difference was observed at 3 months. ARI were significantly different between the groups at all time points. Conclusions: iBOND and G-Bond yielded sufficient SBS’s over the three time points that may be sufficient to withstand occlusal and light archwire forces.en
dc.format.extent1224328 bytes
dc.format.mimetypeapplication/pdf
dc.language.isoengen_US
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectOrthodonticsen
dc.titleShear bond strengths of two new self-etching primersen
dc.typeinfo:eu-repo/semantics/masterThesis
dc.typemaster thesisen_US
dc.degree.disciplinePreventive Dental Scienceen_US
dc.contributor.examiningcommitteeSwain, Vanessa (Restorative Dentistry) Wiltshire, William (Preventive Dental Science)en
dc.degree.levelMaster of Science (M.Sc.)en_US
dc.description.noteOctober 2010en


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record